MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Niche Polymer POLISAV™ TPE50DWT Hytrel, 50D
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes:

Information provided by Niche Polymer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
Filler Content 3.5 %TiO2; ASTM D2584
Moisture Absorption at Equilibrium 0.20 %50% RH; ASTM D570
Melt Flow 18.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 47 - 52ASTM D2240
Tensile Strength at Break 41.0 MPaASTM D638
Tensile Strength, Yield 19.0 MPaASTM D638
Elongation at Break 580 %ASTM D638
Flexural Strength 10.0 MPaASTM D790
Flexural Modulus 235 MPaASTM D790
Izod Impact, Notched (ISO) NBASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 200 °C
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Niche Polymer POLISAV™ TPE45DBK Hytrel, 45D
Celanese Hytrel® 4556 TPC-ET
Celanese Hytrel® G4074 TPC-ET
Celanese Hytrel® 8238 TPC-ET
Celanese Hytrel® 6359FG NC010 TPC-ET

PNICHE116 / 193698

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.