MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay IONQUEST® 290 Bis (2,4,4-Trimethylpentyl) Phosphonic acid
Categories: Fluid

Material Notes: Identification: BIS (2,4,4-TRIMETHYLPENTYL) PHOSPHINIC ACID

CAS: 83411 – 71 – 6

Available in: Asia Pacific, Europe, Latin America and North America

Applications: IONQUEST® 290 is an excellent extractant for separating cobalt from nickel. It will also extract other cations such as aluminum, copper and zinc.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 0.918 g/ccOSTM059
 
Processing PropertiesOriginal ValueComments
Shelf Life 48.0 Month
 
Descriptive Properties
AppearanceClear, colorless to pale yellow liquid
Dry FlowDF-1-1Pass
Purity31P NMR, OPTI061>95% (area)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cesium Hydroxide, CsOH
Petroquimica Triunfo Trithene® SX 7010 LDPE - Blow Molding

WRHOD169 / 137400

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.