MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECAFIL PEEK VX natural - 1,75 mm - Filament Polyetheretherketone
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes:
  • inherent flame retardant
  • very good chemical resistance
  • good slide and wear properties
  • good heat deflection temperature
  • resistance against high energy radiation
  • hydrolysis and superheated steam resistant
Target Industries:
  • electronics
  • food technology
  • automotive industry
  • chemical technology
  • mechanical engineering
  • aircraft and aerospace technology

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.30 g/cc
Moisture Absorption 0.0300 %DIN EN ISO 62
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 380 °C
DIN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 100 MPa50 mm/min; DIN EN ISO 527-1
Elongation at Break 25 %50 mm/min; DIN EN ISO 527-1
Modulus of Elasticity 3.60 GPa50 mm/min; DIN EN ISO 527-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µm/m-°CDIN EN ISO 11359-1;2
Melting Point 343 °CDIN EN ISO 11357
Maximum Service Temperature, Air 260 °Clong term
 300 °Cshort term
Deflection Temperature at 1.8 MPa (264 psi) 162 °CISO-R 75 Method A
Glass Transition Temp, Tg 143 °CASTM D3418
Flammability, UL94 V-0125x13x1,5mm; DIN IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 230 °CBuild chamber temperature
 160 - 250 °CPrint bed temperature
Nozzle Temperature 420 - 440 °CDiameter: 0,4 mm
Melt Temperature <= 470 °C
Drying Temperature 120 °C
Dry Time 8.00 hour
 
Descriptive Properties
Colorbeige opaque
Fan speed0
Print speed20-30 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIO1269 / 319197

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.