MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Petromont 7002 Medium Density Polyethylene Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded; Medium Density (MDPE)

Material Notes: Petromont HDPE 7002 is a medium-density polyethylene hexene modified resin with an excellent balance of chemical resistance and durability. It is designed to be readily processed by flat die extrusion equipment.

Petromont HDPE 7002 is an unpigmented polyethylene compound which, after proper incorporation of carbon black, may be used for geomembrane applications, such as liners for landfills and surface impoundments, where polyethylene is the material of choice. Comprehensive information on such facilities is available in documents issued by the U.S.A EPA.

When Petromont HDPE 7002, containing sufficient stabilizers, is properly processed into sheet, installed and seamed, the resulting liner is expected to provide excellent resistance to aqueous chemicals and solvents as well as to stress cracking. Sheet made in this way from Petromont HDPE 7002 can be expected to pass the physical property requirements of the GM-13 of GRI (Geosynthetic Research Institute) for Flexible Membrane Liners.

Key Words: Geomembrane, Cast Line Grade
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.9375 g/ccASTM D1505
Environmental Stress Crack Resistance >= 2000 hourF0; ASTM D1693/B
Oxidative Induction Time (OIT) >= 100 min200°C with oxygen in aluminum pan; ASTM D3895
Melt Flow 0.20 g/10 minI2; ASTM D1238/E
 20 g/10 minI21; ASTM D1238/F
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 31.0 MPaASTM D638
Tensile Strength, Yield 20.0 MPaASTM D638
Elongation at Break >= 850 %ASTM D638
Flexural Modulus 0.650 GPaASTM D790
 
Descriptive Properties
ProcessExtrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® HHM TR-305 Medium density hexene copolymer
Petromont 2100 Medium Density Polyethylene Resin
Borealis Borstar® FB1350 Medium Density Polyethylene
Bayport Polymers Baystar™ Lumicene® mPE M 3410 EP MDPE Film, sheet
Bayport Polymers Baystar™ Lumicene® mPE BM 359 SG Metallocene Medium Density High Gloss Blow Molding Resin

PPETROM22c / 56217

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.