MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals ARCEL® ULV Expanded Polyethylene/Styrenic Polymer
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: ARCEL ULV resin can be continuously or batch expanded using conventional EPS expansion equipment. Some minor material handling modifications may be required. ACREL ULV resin has been expanded in continuous expanders ranging in size from 210 to 1,125 liters (55 to 300 gallons) as well as several sizes of batch expanders.

NOVA Chemicals' ARCEL resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0160 g/ccContinuous - Double Pass, Pre-puff Density
 0.0176 g/ccContinuous - Double Pass, Foam Density
 0.0208 g/ccBatch - Single Pass, Pre-puff Density
 0.0232 g/ccBatch - Single Pass, Foam Density
 0.0240 g/ccContinuous - Single Pass, Pre-puff Density
 0.0272 g/ccContinuous - Single Pass, Foam Density
Filler Content 0.30 %Plasticizer
 5.5 %Pentane
Particle Size 900 - 2000 µmDiameter; 98% of particles
Storage Temperature <= 4.00 °CIndefinite shelf life expected at this temperature or lower.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 41.7 psi1.25 pcf; ASTM D 3575
 51.7 psi1.50 pcf; ASTM D 3575
 60.9 psi1.75 pcf; ASTM D 3575
 69.3 psi2.00 pcf; ASTM D 3575
 83.5 psi2.50 pcf; ASTM D 3575
 94.3 psi3.00 pcf; ASTM D 3575
 102 psi3.50 pcf; ASTM D 3575
 106.3 psi4.00 pcf; ASTM D 3575
Flexural Strength 39.6 psiat Max Load; 1.25 pcf; ASTM-C203
 51.1 psiat Max Load; 1.5 pcf; ASTM-C203
 62.1 psiat Max Load; 1.75 pcf; ASTM-C203
 72.4 psiat Max Load; 2 pcf; ASTM-C203
 91.1 psiat Max Load; 2.5 pcf; ASTM-C203
 107.3 psiat Max Load; 3 pcf; ASTM-C203
 121 psiat Max Load; 3.5 pcf; ASTM-C203
 132.2 psiat Max Load; 4 pcf; ASTM-C203
 34.9 psi
@Strain 5.0 %
1.25 pcf; ASTM-C203
 46.0 psi
@Strain 5.0 %
1.5 pcf; ASTM-C203
 56.6 psi
@Strain 5.0 %
1.75 pcf; ASTM-C203
 66.6 psi
@Strain 5.0 %
2 pcf; ASTM-C203
 85.0 psi
@Strain 5.0 %
2.5 pcf; ASTM-C203
 101.4 psi
@Strain 5.0 %
3 pcf; ASTM-C203
 115.6 psi
@Strain 5.0 %
3.5 pcf; ASTM-C203
 127.7 psi
@Strain 5.0 %
4 pcf; ASTM-C203
Flexural Strain at Break 6.9 %Flexural Strain; at Max Load; 4 pcf; ASTM-C203
 7.7 %Flexural Strain; at Max Load; 3.5 pcf; ASTM-C203
 8.4 %Flexural Strain; at Max Load; 3 pcf; ASTM-C203
 9.2 %Flexural Strain; at Max Load; 2.5 pcf; ASTM-C203
 9.9 %Flexural Strain; at Max Load; 2 pcf; ASTM-C203
 10.3 %Flexural Strain; at Max Load; 1.75 pcf; ASTM-C203
 10.7 %Flexural Strain; at Max Load; 1.5 pcf; ASTM-C203
 11.1 %Flexural Strain; at Max Load; 1.25 pcf; ASTM-C203
Compressive Strength 16.5 psi
@Strain 10 %
1.25 pcf; ASTM-D3575
 19.1 psi
@Strain 25 %
1.25 pcf; ASTM-D3575
 20.9 psi
@Strain 10 %
1.50 pcf; ASTM-D3575
 24.3 psi
@Strain 25 %
1.50 pcf; ASTM-D3575
 25.4 psi
@Strain 10 %
1.75 pcf; ASTM-D3575
 27.7 psi
@Strain 50 %
1.25 pcf; ASTM-D3575
 29.4 psi
@Strain 25 %
1.75 pcf; ASTM-D3575
 29.9 psi
@Strain 10 %
2.00 pcf; ASTM-D3575
 33.3 psi
@Strain 50 %
1.50 pcf; ASTM-D3575
 34.5 psi
@Strain 25 %
2.00 pcf; ASTM-D3575
 38.8 psi
@Strain 10 %
2.50 pcf; ASTM-D3575
 39.0 psi
@Strain 50 %
1.75 pcf; ASTM-D3575
 44.6 psi
@Strain 50 %
2.00 pcf; ASTM-D3575
 44.8 psi
@Strain 25 %
2.50 pcf; ASTM-D3575
 47.8 psi
@Strain 10 %
3.00 pcf; ASTM-D3575
 55.1 psi
@Strain 25 %
3.00 pcf; ASTM-D3575
 55.8 psi
@Strain 50 %
2.50 pcf; ASTM-D3575
 56.7 psi
@Strain 10 %
3.50 pcf; ASTM-D3575
 59.7 psi
@Strain 75 %
1.25 pcf; ASTM-D3575
 65.3 psi
@Strain 25 %
3.50 pcf; ASTM-D3575
 65.7 psi
@Strain 10 %
4.00 pcf; ASTM-D3575
 67.0 psi
@Strain 50 %
3.00 pcf; ASTM-D3575
 71.0 psi
@Strain 75 %
1.50 pcf; ASTM-D3575
 75.6 psi
@Strain 25 %
4.00 pcf; ASTM-D3575
 78.2 psi
@Strain 50 %
3.50 pcf; ASTM-D3575
 82.3 psi
@Strain 75 %
1.75 pcf; ASTM-D3575
 89.5 psi
@Strain 50 %
4.00 pcf; ASTM-D3575
 93.6 psi
@Strain 75 %
2.00 pcf; ASTM-D3575
 116.2 psi
@Strain 75 %
2.50 pcf; ASTM-D3575
 138.8 psi
@Strain 75 %
3.00 pcf; ASTM-D3575
 161.4 psi
@Strain 75 %
3.50 pcf; ASTM-D3575
 183.9 psi
@Strain 75 %
4.00 pcf; ASTM-D3575
Puncture Energy 37.8 ft-lb
 44.6 ft-lb
 51.9 ft-lb
 59.8 ft-lb
 77.3 ft-lb
 97.1 ft-lb
 119.2 ft-lb
 143.6 ft-lb
Tear Strength 1.47 kN/m1.25 pcf; ASTM D 3575
 1.81 kN/m1.50 pcf; ASTM D 3575
 2.16 kN/m1.75 pcf; ASTM D 3575
 2.51 kN/m2.00 pcf; ASTM D 3575
 3.21 kN/m2.50 pcf; ASTM D 3575
 3.89 kN/m3.00 pcf; ASTM D 3575
 4.59 kN/m3.50 pcf; ASTM D 3575
 5.29 kN/m4.00 pcf; ASTM D 3575
 
Descriptive Properties
ColorWhite
ShapeSpherical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOVB111 / 194719

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.