MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
3M Scotch® 8919MSR Filament Tape
Categories: Polymer; Adhesive

Material Notes: Scotch® Filament Tape 8919MSR is a high-performance transparent filament tape reinforced along its length with continuous fiberglass-yarn filaments, which gives the tape a very high tensile strength. The tape is designed to hold a variety of metal appliance parts together during manufacture and shipping. The heavy clear polyester film backing provides greater stiffness and excellent abrasion, moisture, and scuff resistance. The pressure sensitive modified synthetic rubber resin adhesive is specifically formulated to provide high adhesion to oily metal surfaces, clean removal, and stain resistance on a wide variety of surfaces.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 7.00 milASTM D3652
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 36.9 MPaASTM D3759
Elongation at Break 3.0 %ASTM D3759
Peel Strength 6.5625 pliAdhesion to Steel; ASTM D3330
 
Descriptive Properties
Adhesive TypePressure sensitive modified synthetic rubber resin
AppearanceClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM34192 / 168939

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.