MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm ACRYLITE® Resist wave profile Graphite Grey Prismatic 7RW02 Acrylic, Extruded
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Extruded

Material Notes: Available Forms: Wave Profile
Masking: Other
Properties: Impact Resistant; UV Filtering
Optical Properties: Translucent; UV Filtering
Surface: Prismatic
Weatherability: Indoor; Outdoor
Sizes: 41.14” x 192.9”
Thicknesses: 0.118”
Wavelength / Amplitude: 2.992” / 0.709”
Applications: Architectural and Decorative Lighting Fixtures; Carports; Commercial Greenhouse; Dividers and Decorative Panels; Hobby and Residential Greenhouse; Institutional Greenhouse; Patio and Deck Covers; Research Greenhouse; Retail Greenhouse |Roof Panels; Skylights and Daylighting: Wall Panels: Zoo Enclosures

Information provided by Roehm America LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 66 %
 
Descriptive Properties
ColorGraphite Grey Prismatic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PROHM9035 / 319652

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.