A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has controlled rheology for robotic or specialty extrusion applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for extrusion. It is polyolefin based and completely recyclable. Key Features: - Designed for applications requiring good elastic recovery.
- Designed for improved UV resistance.
- Recommended for applications requiring superior part surface appearance.
Applications:Uses:- Automotive Applications
- Automotive Exterior Trim
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical |
EU 2003/11/EC; RoHS Compliant |