MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 218HP V35 Black 21N PA 66 35% Glass Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Description: TECHNYL® A 218HP V35 Black 21N is a polyamide 6.6, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in black color.

Key Properties: Excellent combination between thermal & mechanical properties; Long term stability up to 190°C in air; Higher lifetime after heat ageing

Benefits: The product offers an outstanding long term heat resistance and is suitable to work in environments characterized by a very high temperature.

Applications: It is used in a wide variety of industries, especially in automotive industry for air circuit parts such as intercoolers

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccISO 1183/A
Linear Mold Shrinkage 0.0077 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0046 cm/cm
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 107 MPaISO 527 Type 1A
Elongation at Break 5.6 %ISO 527 Type 1A
Tensile Modulus 7000 MPaISO 527 Type 1A
Charpy Impact Unnotched 75.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 18.0 kJ/m²ISO 179/1eA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOLVAY841 / 218569

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.