MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Thermal Ceramics FireMaster FP-60 Blanket
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: FireMaster Blanket is a high-temperature fiber blanket which is classified by Underwriters Laboratories under “Batts and Blankets (BKNV)” in the UL Building Materials Directory, No. R8418. FireMaster Blanket is manufactured to ensure continued compliance with certification standards. The blanket is used as a fireproof covering or wrap. Foil facing or encapsulation is available in aluminum or stainless steel to reduce the risk of physical damage, minimize dusting, and protect against weathering.

Features:

  • UL-classified, noncombustible material
  • Lightweight/flexible
  • Optional foil facing or encapsulation
  • Low thermal conductivity
  • Resists chemical attack
  • Unaffected by oil or water
  • Completely inorganic
  • Excellent acoustical properties
  • Applications:

  • OEM manufactured systems such as fire doors and panels
  • Up to 3 hour cable tray, conduit, and through penetration firestops
  • Structural steel
  • Plastic pipes
  • Above ground storage tanks
  • Railcar tanks
  • Motor Operated Valves
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Thermal PropertiesOriginal ValueComments
    Thermal Conductivity 0.210 BTU-in/hr-ft²-°F
    @Temperature 37.8 °C
     0.440 BTU-in/hr-ft²-°F
    @Temperature 260 °C
     0.870 BTU-in/hr-ft²-°F
    @Temperature 538 °C
     1.45 BTU-in/hr-ft²-°F
    @Temperature 816 °C
     2.09 BTU-in/hr-ft²-°F
    @Temperature 1090 °C
    Melting Point 3200 °F
    Maximum Service Temperature, Air 2300 °F
    Flammability Test 0.00Flame Spread
     0.00Smoke Developed
     0.00Fuel Contributed
     
    Component Elements PropertiesOriginal ValueComments
    Al2O3 45 %
    Other 2.0 %
    SiO2 53 %
     
    Descriptive Properties
    Water Leachable Elements on Surface of Fiber, PPMBoron, 100
     Chlorine, 5
     Fluorine, <5
     Sulfur, 10

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Industrial Nanotech Nansulate™ GP Translucent Insulation Coating
    Flakeboard

    CTHERM111 / 2431

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.