MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik 19.9.LSi Welding wire
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 19.9.LSi is a filler metal particularly suited for MIG welding. It can also be used for TIG and plasma arc welding. It is suitable for joining stainless steels of the 18Cr/8Ni ELC type and 18Cr/8Ni/Nb type for service temperatures up to 350°C (660°F).

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 160
Tensile Strength, Ultimate 440 MPa
@Temperature 400 °C
 600 MPa
@Temperature 20.0 °C
Tensile Strength, Yield 290 MPa
@Strain 0.2 %,
Temperature 400 °C
 390 MPa
@Strain 0.2 %,
Temperature 20.0 °C
Elongation at Break 24 %
@Temperature 400 °C
 42 %
@Temperature 20.0 °C
Reduction of Area 60 %
Charpy Impact 50.0 J
@Temperature -196 °C
 120 J
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 400 °C
Thermal Conductivity 15.0 W/m-K
@Temperature 20.0 °C
 16.0 W/m-K
@Temperature 100 °C
 19.0 W/m-K
@Temperature 300 °C
 21.0 W/m-K
@Temperature 500 °C
Maximum Service Temperature, Air 350 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.020 %All-Weld Metal
 <= 0.025 %AIM
Chromium, Cr 20 %AIM
 20 %All-Weld Metal
Manganese, Mn 1.6 %All-Weld Metal
 1.8 %AIM
Molybdenum, Mo <= 0.30 %AIM
Nickel, Ni 10.5 %AIM
 10.5 %All-Weld Metal
Nitrogen, N <= 0.060 %AIM
 <= 0.060 %All-Weld Metal
Phosphorus, P 0.010 %All-Weld Metal
 <= 0.025 %AIM
Silicon, Si 0.80 %All-Weld Metal
 0.90 %AIM
Sulfur, S 0.011 %All-Weld Metal
 <= 0.015 %AIM

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSANDV5098 / 199662

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.