MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Ethydco Advancene™ EM-5333-AAH HDPE Blow Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Blow molding. A multipurpose polymer designed for high speed production of blow molded containers used to package household industrial chemicals, toiletries, and cosmetics, health and medical aids, and food products. In addition, it can be blow molded into other thin walled parts and houseware items, and can be extruded into profiles. Main characteristics: excellent environmental stress crack resistance and rigidity, high impact strength, moderate swell, high melt strength.

Mechanical property data for samples molded and tested in accordance with ASTM D4976.

Information provided by ETHYDCO.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.953 g/ccASTM D792
ESCR 100% Igepal® 80 hour
@Temperature 50.0 °C
F50; ASTM D1693
High Load Melt Index 33 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238, ISO 1133
Melt Index of Compound 0.38 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238, ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 61ASTM D2240, ISO/IEC 17025:1999
Tensile Strength at Break 31.0 MPaASTM D638, ISO 527
Tensile Strength, Yield 26.9 MPaASTM D638, ISO 527
Elongation at Break 1000 %ASTM D638, ISO 527
Elongation at Yield 7.0 %ASTM D638, ISO 527
2% Secant Modulus 1000 MPaASTM D790B, ISO 178,
Tensile Impact Strength 168 kJ/m²Type S; ASTM D1822, ISO 8256
 
Thermal PropertiesOriginal ValueComments
Melting Point 131 °CASTM D3418, ISO 3146
Crystallization Temperature 118 °CASTM D3418, ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °CUnannealed; ASTM D648, ISO 75
Vicat Softening Point 129 °CASTM D1525, ISO 306
Brittleness Temperature <= -76.0 °CASTM D746, ISO 974( E)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil HD 6719.17 High Density Polyethylene Copolymer Resin
ICO Polymers ICOFLO™ 510-5007 1200 Micron HDPE Powder
Kazanorgsintez PE2NT26-13 High Density Polyethylene Composite
ExxonMobil Paxon™ AS55-003 Blow Molding Resin
ExxonMobil Paxon™ AM55-003 Blow Molding Resin

PETHYD904 / 200050

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.