Product Description: A black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-12 for applications such as co-extruded, thermoformed automotive coolant hose. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable. Key Features: - Designed for excellent adhesion to PA-12 even after thermoforming of co-extruded corrugated tubes.
- EU and China RoHS compliant.
Information provided by ExxonMobil Chemical. |