MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
International Mold Steel Superplast® Stainless Plastic and Rubber Mold Steel
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: Superplast Stainless is a prehardened, free-machining, stainless mold steel specially designed for plastic mold bases. It also provides improved performances compared to standard grades such as W1.2085. Superplast Stainless offers: Improved machinability; Improved consistency and weldability

Information provided by International Mold Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 310
Tensile Strength, Ultimate 1000 MPa
Tensile Strength, Yield 890 MPa
Elongation at Yield 14 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.070 %
Chromium, Cr 12 %
Iron, Fe >= 87.83 %
Silicon, Si 0.10 %
Sulfur, S <= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Fluoroelastomer
Polybutadiene Rubber (BR)
Mitsubishi Chemical Advanced Materials Nylatron® SLG-FDA PA6 (ASTM Data Sheet)
Mitsubishi Chemical Advanced Materials Semitron® ESd 520HR (ASTM Product Data Sheet)
Overview of materials for Thermoset Polyurethane, Elastomer, Glass Filled

NIMSA01 / 175981

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.