System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Wanhua Chemical Wanthane® WHT-8180 Polyether-Based TPU
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Polyurethane TPE
;
Polyurethane, TP
;
Thermoplastic Polyurethane (TPUR), Polyether Grade
Material Notes:
Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistance
Information provided by Wanhua Chemical Group Co., Ltd.
Key Words:
FDA 21 CFR 177.1680, 177.2600; USP VI
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.10
g/cc
ASTM D792
Mechanical Properties
Original Value
Comments
Hardness, Shore A
80
ASTM D2240
Tensile Strength
25.0
MPa
ASTM D412
Elongation at Break
600 %
ASTM D412
100% Modulus
0.00600
GPa
@Strain 100 %
ASTM D412
300% Modulus
0.0100
GPa
@Strain 300 %
ASTM D412
Tear Strength
75.0
kN/m
ASTM D624
Thermal Properties
Original Value
Comments
Glass Transition Temp, Tg
-45.0
°C
Processing Properties
Original Value
Comments
Processing Temperature
175
-
190
°C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Taiwan PU Corporation UR50 Polyester Urethane Rubber
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer
Celanese Ateva® 2803G Ethylene Vinyl Acetate Copolymer
Westlake Plastics Pomalux® Acetal Copolymer, Compression Molded
Huntsman IROGRAN® A 75 P 4665N TPU-Polyether
PWANTH953 / 156376
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.