MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® UV8800M Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Appearance: Medium grey paste

Cure: Ultraviolet (UV) light

Product Benefits:

  • One component
  • Medium viscosity
  • Cures rapidly
  • Low shrinkage
  • Excellent adhesion
Application: Encapsulant

Typical Package Application: Chip scale packages and BGA

Substrates: Glass, Epoxy, Polyimide and Polyester

LOCTITE UV8800M epoxy encapsulant is developed to meet high temperature thermal cycling specifications. It cures to form a hard translucent coating when exposed to UV light of sufficient intensity. The curing of the product is not inhibited by oxygen, resulting in excellent surface cure. Its viscosity characteristics and dearated condition make it suitable for accurate dispensing with excellent shape control.

Information provided by Loctite®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.60 g/cc
Filler Content 53.6 %
Water Absorption 0.90 %
@Time 86400 sec
Particle Size 5.0 µmD50
 21 µmD95
Viscosity 2500 - 4000 cPUncured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78Cured
Tensile Modulus 2850 MPaCured, DMA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 41.0 µm/m-°CCured, Below Tg
 135 µm/m-°CCured, Above Tg
Glass Transition Temp, Tg 29.0 °CCured
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 0.000 - 5.00 °C
 
Descriptive Properties
Extractable Ionic Content (ppm)237Cured, Fluoride (F-), MIL-S-883
 34Cured, Chloride (Cl-), MIL-S-883

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOCT5106 / 255317

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.