MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound LC006 Polyetheretherketone (PEEK) (Americas)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: LNP THERMOCOMP LC006 compound is based on Polyetheretherketone (PEEK) resin containing 30% carbon fiber. Added features of this grade include: Electrically Conductive.

Features: High Stiffness,Light-weight Structural,High Heat Resistance,Super Strong (Carbon Fiber Filled),Electrically Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccISO 1183
 1.413 g/ccASTM D792
Moisture Absorption 0.0700 %23°C / 50% RH; ISO 62
 0.0800 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0010 cm/cm24hrs; ASTM D955
 0.0012 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0040 cm/cm24hrs; ASTM D955
 0.0040 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 225 MPaASTM D638
 230 MPaISO 527
Elongation at Break 1.5 %ASTM D638
 1.5 %ISO 527
Tensile Modulus 24050 MPa1 mm/min; ISO 527
 30750 MPa50 mm/min; ASTM D638
Flexural Strength 325 MPaASTM D790
 346 MPaISO 178
Flexural Modulus 20200 MPaASTM D790
 24300 MPaISO 178
Izod Impact Notched 74.0 JASTM D256
Izod Impact, Unnotched 608 J/mASTM D4812
Izod Impact, Notched (ISO) 9.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 44.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 12.0 Jpeak; ASTM D3763
Coefficient of Friction, Dynamic 0.30ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.32ASTM D3702 Modified: Manual
K (wear) Factor 55.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 12.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 12.1 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 29.3 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 29.3 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 298 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 300 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 298 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 0.770 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 380 - 400 °C
Zone 3 380 - 400 °C
Mold Temperature 175 - 190 °C
Drying Temperature 150 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa
Screw Speed 60 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81667 / 289614

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.