MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lubrizol LifeSciences Pellethane® 5855-92A TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Aromatic Polyester-based Thermoplastic Polyurethane (TPU)

Features: Good physical properties, good chemical resistance, and a wide processing window for extrusion.

Process: Extrusion and Injection Molding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 92ASTM D2240
Tensile Strength, Ultimate 9000 psiASTM D412
Elongation at Break 450 %ASTM D412
100% Modulus 9.70 MPa
@Strain 100 %
ASTM D412
300% Modulus 29.9 MPa
@Strain 300 %
ASTM D412
Tear Strength 33.3 kN/mTrouser; ASTM D470
Graves Tear Strength 650 plidie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 50
@Load 1.00 kg
H-18; ASTM D3389
Tensile Set 20 %
@Temperature 200 °C
ASTM D412
 
Thermal PropertiesOriginal ValueComments
Melting Point 130 °CKofler
 140 °C
Glass Transition Temp, Tg -20.0 °C
 
Optical PropertiesOriginal ValueComments
Haze 1.1 %
@Thickness 1.65 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 188 °CInjection Molding
Front Barrel Temperature 193 °CInjection Molding
Nozzle Temperature 199 °CInjection Molding
Zone 1 177 °CExtrusion
Zone 2 182 °CExtrusion
Zone 3 188 °CExtrusion
Zone 4 193 °CExtrusion
Adapter Temperature 199 °CExtrusion, 5
Die Temperature 199 °CExtrusion
 199 °CExtrusion, 2
Melt Temperature 199 °CInjection Molding
Mold Temperature 21.0 °CInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Pellethane® 2363-55D TPU
Lubrizol LifeSciences Pellethane® 5863-91A TPU
Lubrizol LifeSciences Pellethane® 2363-80A TPU
Lubrizol Pellethane® 2363-90AE Thermoplastic Polyurethane Elastomer
Lubrizol Pellethane® 2363-55DE Thermoplastic Polyurethane Elastomer

PLUBR9041 / 203608

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.