MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Persian Gulf Polymer LDPE – LFI2125A
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: LFI 2125A is suitable for packaging films and is especial suitable when ultimate down gauging is required. Processing Method: LFI 2125A is a grade with a very high level of anti-block and a high level of slip agent (Erucamide) the grade has an excellent draw down ability. The films produced from this grade are stiff, have excellent optical properties, low COF and no blocking. Additive: Antioxidant, slip agent, anti-blocking agent.

Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.921 g/ccISO 1183 (A)
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 13.0 MPaISO 527
Film Tensile Strength at Yield, TD 11.0 MPaISO 527
Film Elongation at Break, MD 100 %ISO 527
Film Elongation at Break, TD >= 500 %ISO 527
Secant Modulus, TD 0.180 GPa2% Secant; ISO 527
Tensile Impact 230 J/cmASTM D4272
Tear Strength 25.0 kN/mTD; ISO 6383-2
 70.0 kN/mMD; ISO 6383-2
Film Tensile Strength at Break, MD 30.0 MPaISO 527
 190 MPaISO 527
Film Tensile Strength at Break, TD 19.0 MPaISO 527
 
Optical PropertiesOriginal ValueComments
Haze <= 9.0 %ASTM D1003 A
Gloss 60 %45°; ASTM D2457
 
Descriptive Properties
Blocking<5 gSABTEC Method
Re-blocking0gSABTEC Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPERSI964 / 250368

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.