MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ITW Devcon® HP 250 Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: High performance epoxy with high shear strength and impact toughness for structural assembly applications. Uses: Bonds metals, FRP/SMC composites, phenolics, stainless steel, aluminum, vinyl esters, nylon, PVC, PC, styrenics, wood, and rigid plastics. Features: Non-corrosive/outstanding chemical resistance, Excellent salt spray durability.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0392 lb/in³
 9.00 lb/galuncured
Solids Content 100 %
Viscosity 75000 cPHardener
 105000 cPMixed
 120000 cPResin
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78
Elongation at Break 25 %
Adhesive Bond Strength 3200 psi[GBS] @ 0.01" bondline. Cured 7 days @ 75°F. Lap Shear; ASTM D1002
Impact Test 12.3 ft-lb
Peel Strength 35.0 - 40.0 pliASTMf D1876
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 19.3 kV/mm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -67.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 168 hourFull
 24.0 hour
@Temperature 24.0 °C
Functional cure
 168 hour
@Temperature 24.0 °C
As Tested
Pot Life 65.0 min
@Temperature 22.2 °C
 
Descriptive Properties
Chemical/Solvent ResistanceAcetic Acid (diluted) 10%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Ammonia: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Cutting oil: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Ethanol: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Gasoline (unleaded): poor30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric Acid 10%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Isopropanol: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Mineral Spirits 10%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Motor Oil: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hypochlorite: Excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
ColorStrawUncured
Gap Filling (in)Excellent
Mix Ratio by volume2:1
Mix Ratio by weight100:42
Specific Volume (in.³/lb)25.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWD9220 / 239729

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.