MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Benzoflex™ 1046 Plasticizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Benzoflex™ 1046 is a specialty benzoate plasticizer imparting excellent stain resistance in PVC or PVC acetate copolymers. Its high resin solvation at elevated temperatures, coupled with its tolerance for fillers, makes it the plasticizer of choice for wall coverings and vinyl floor coverings. In addition, its excellent rheological properties make it highly desirable for plastisol and organosol applications.

Application/Uses:

  • Automotive
  • Flooring/Interior surfaces
  • PVC plastisol sealant

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/cc
Viscosity 52 cP
Vapor Pressure 0.00000120 atm
 
Thermal PropertiesOriginal ValueComments
Melting Point <= -34.0 °CFreezing Point
Boiling Point 346 °C
Flash Point 170 °CSetaflash Closed Cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.492
 
Descriptive Properties
ColorPt-Co

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTINOL® INB Plasticizer
Evonik VESTINOL® 9 Plasticizer
Evonik Modifier OH 650 Plasticizer
Evonik Modifier 715 Plasticizer
Evonik Modifier 705 Plasticizer

PEATM5077 / 222271

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.