PA66 for injection molding, flame retarded with non halogen flame retardant, heat stabilized. Main features: flammability in accordance with UL 94 V2 at 1,6 mm, glow wire at 960°C at 1,1 mm. Application for the electrical industry: protectors, coil forms, covers, terminals. Delivered in natural or in grey. Application: Injection molding. Information Provided by Plastcom spol. s r.o. |