MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Kraton® A1535 H (SEBS) Linear Triblock Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton A1535 H is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 57%. It is supplied from North America in the physical form identified:
Kraton A1535 HU - supplied as an undusted powder
Kraton A1535 HS - supplied as a dusted powder

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton A1535 H is used as a base material for compound formulations and as a modifier of thermoplastics. The inherent stability of the mid block suggests the use of this product in applications that must withstand weathering and high processing temperatures.

Applications: Compounding and Personal Hygiene

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 1.0 %KM 04
Melt Flow <= 1.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 83
@Time 10.0 sec
ASTM D2240
Tensile Strength 27.6 MPaMeasured on solution cast film from toluene; BAM 1245
Elongation at Break >= 600 %Measured on solution cast film from toluene; BAM 1245
300% Modulus 0.00793 GPa
@Strain 300 %
Measured on solution cast film from toluene; BAM 1245
 
Descriptive Properties
ContentNon-staining phenolic antioxidant0.03-0.1%, KM 08
 Polystyrene56.3-60.3%, Measured on the polymer before hydrogenation, KM 03
 Total Extractables<1.6%, KM 05

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® A1536 H (SEBS) Linear Triblock Copolymer
Kraton® D1193 P (SIS) Linear Triblock Copolymer
Kraton® D1124 B (SIS) Branched Triblock Copolymer
Kraton® D1126 P (SIS) Radial Copolymer
Kraton® D1160 E (SIS) Linear Triblock Copolymer

PKRA9882 / 132781

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.