MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ FR BFL2015 PC (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN BFL2015 Polycarbonate (PC) is an injection moldable non-chlorinated/brominated flame retardant grade that is 15% glass fiber filled and has improved flow. It has a UL94 V0@1.5mm rating and is available in various opaque color options.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccASTM D792
Density 1.30 g/ccISO 1183
Water Absorption 0.35 %23°C/sat; ISO 62
Moisture Absorption 0.150 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cmSABIC method
 0.0020 - 0.0050 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0020 - 0.0050 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 6.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
cm³/10 min; ISO 1133
 6.5 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 91.0 MPa50 mm/min; ASTM D638
 100 MPa50 mm/min; ISO 527
Tensile Strength, Yield 92.0 MPa50 mm/min; ASTM D638
 103 MPa50 mm/min; ISO 527
Elongation at Break 4.0 %50 mm/min; ASTM D638
 4.3 %50 mm/min; ISO 527
Elongation at Yield 3.5 %50 mm/min; ASTM D638
 3.6 %50 mm/min; ISO 527
Tensile Modulus 4950 MPa1mm/min; ISO 527
 5330 MPa5 mm/min; ASTM D638
Flexural Yield Strength 150 MPa2 mm/min; ISO 178
 156 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 4280 MPa2 mm/min; ISO 178
 4600 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 78.0 J/mASTM D256
 NB
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 8.00 kJ/m²80*10*3; ISO 180/1A
 7.00 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) 80.0 kJ/m²80*10*3; ISO 180/1U
 80.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Charpy Impact Unnotched 67.0 kJ/m²ISO 179/2C
 100 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eU
 75.0 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
 100 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 12.0 kJ/m²ISO 179/2C
 6.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
 8.00 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
Dart Drop, Total Energy 61.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 3.1
@Frequency 1e+6 Hz
IEC 60250
 3.2
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 20.0 kV/mm
@Thickness 1.60 mm
in oil; ASTM D149
Dissipation Factor 0.010
@Frequency 1e+6 Hz
IEC 60250
 0.020
@Frequency 50.0 - 60.0 Hz
IEC 60250
Comparative Tracking Index 150 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
 40.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 40.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 40.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Hot Ball Pressure Test 125 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 141 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 148 °CRate B/50; ASTM D1525
 149 °CRate B/50; ISO 306
 150 °CRate B/120; ISO 306
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
UL 94
Oxygen Index 38 %ISO 4589
Glow Wire Test 825 °C
@Thickness 1.00 mm
IEC 60695-2-13
 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Nozzle Temperature 280 - 310 °CInjection Molding
Zone 1 270 - 300 °C
Zone 2 280 - 310 °C
Zone 3 290 - 320 °C
Melt Temperature 290 - 320 °C
Mold Temperature 80.0 - 120 °C
Drying Temperature 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10629 / 244096

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.