MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Aleris HOGAL 5558 Aluminum 5026 H14/H34
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: HOGAL 5558 is produced according to EN AW-5026.

Information provided by Aleris.

Key Words: AlMg4.5MnSiFe; Composition per EN 573-3:2009-08
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.66 g/ccAA 5083
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 88
@Thickness 5.00 - 12.0 mm
Typical
 52
@Thickness 5.00 mm,
Temperature 200 °C
Calculated
 64
@Thickness 5.00 mm,
Temperature 150 °C
Calculated
 84
@Thickness 5.00 mm,
Temperature 100 °C
Calculated
 87
@Thickness 5.00 mm,
Temperature 25.0 °C
Tensile Strength, Ultimate >= 250 MPaGuaranteed Minimum L-T Direction
 290 MPa
@Thickness 5.00 - 12.0 mm
Typical L-T Direction
 170 MPa
@Thickness 5.00 mm,
Temperature 200 °C
Typical L-T Direction
 211 MPa
@Thickness 5.00 mm,
Temperature 150 °C
Typical L-T Direction
 279 MPa
@Thickness 5.00 mm,
Temperature 100 °C
Typical L-T Direction
 292 MPa
@Thickness 5.00 mm,
Temperature 25.0 °C
Typical L-T Direction
Tensile Strength, Yield >= 200 MPaGuaranteed Minimum L-T Direction; 0.2% Offset
 230 MPa
@Thickness 5.00 - 12.0 mm
Typical L-T Direction; 0.2% Offset
Elongation at Break >= 10 %Guaranteed Minimum L-T Direction, in 2 inches
 14 %
@Thickness 5.00 - 12.0 mm
Typical L-T Direction, in 2 inches
Bend Radius, Minimum 3.5 t
@Thickness 5.00 mm
 4.0 t
@Thickness 8.00 mm
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 88.3 - 94.6 %as balance
Chromium, Cr <= 0.30 %
Copper, Cu 0.10 - 0.80 %
Iron, Fe 0.20 - 1.0 %
Magnesium, Mg 3.9 - 4.9 %
Manganese, Mn 0.60 - 1.8 %
Silicon, Si 0.55 - 1.4 %
Titanium, Ti <= 0.20 %
Zinc, Zn <= 1.0 %
Zirconium, Zr <= 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DWA 6092/SiC/17.5p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC), Sheet
DWA 6092/SiC/25p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC), Extruded
304 Stainless Steel
Aleris HOGAL 5558 Aluminum 5026-O/H111
Aluminum 5456-H111

NALERIS91 / 159716

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.