MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Von Roll Delglas® M10 Epoxy - Glass Threaded Rod
Categories: Polymer; Thermoset; Epoxy

Material Notes: Delglas are fastening elements machined from different special grades of epoxy glass laminates. Delglas fastening elements are electrical insulation materials with high dielectric strength, a very good tracking resistance, and strong mechanical properties. They offer excellent resistance to humidity, seawater corrosion and chemical agents avoiding frequent and costly maintenance (rust, painting). They are well adapted for operating in oil and in other dielectric liquids, and at both very low and high temperatures up to 180°C. Delglas fastening elements are used in: Transformers, coils, rectifiers, switches, Generators, rotating machines, Equipment for the chemical industry, Pipelines and gaskets fixations, Marine, oil and gas.

Information provided by Von Roll.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Tensile Strength of Threads (Nm)1230023°C, Nuts H= 1D, threaded rods without flats 68835.
 15500155°C, Nuts H= 2D, threaded rods without flats 68835.
 2200023°C, Nuts H= 2D, threaded rods without flats 68835.
 8000155°C, Nuts H= 1D, threaded rods without flats 68835.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PVONR9935 / 249225

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.