Characteristics: Properties:- Excellent wear and tear resistance
- Superior tensile strength & elongation
- Good solvent resistance
- Low compression set
Comments:- Suitable for forklift tires, sheet goods, wheels, & rollers
- Suitable for sprocket wheels & die-cut pads
- Ideal for gaskets & seals
- Excellent general purpose elastomer
- Improved temperature resistance with HQEE
Information provided by Covestro |