MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos B54-25H-127 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: B54-25H-127 is a high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which require a combination of high top load strength and good environmental stress crack resistance (ESCR). This material contains a fully FDA sanctioned antistat and meets Food and Drug Administration requirements of 21CFR 177.1520.

Key Words: Excellent ESCR and stiffness, good top load, and antistat
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.955 g/ccASTM D4883
Melt Flow 0.35 g/10 minASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
Tensile Strength, Yield 27.6 MPa2 in/min (50 mm/min); ASTM D-638
Elongation at Break 700 %2 in/min (50 mm/min); ASTM D-638
Modulus of Elasticity 1.497 GPaASTM D638
Flexural Modulus 0.690 GPaASTM D747
 1.241 GPaTangent; ASTM D 790
Izod Impact, Notched 1.90 J/cmASTM D256
Tensile Impact Strength 277 kJ/m²ASTM D1822
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °CASTM D648
Vicat Softening Point 131 °CASTM D1525
Brittleness Temperature <= -75.0 °CASTM D746
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
processBlow Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos B53-35H-011 HDPE
Ineos K50-10-136 HDPE
Total PPC 8780 Polypropylene, Heterophasic Copolymer, Injection Molding
Borealis MG9641B Polyethylene
Borealis Bormed™ HE2581-PH HDPE for Healthcare Applications

PSOLK5 / 68212

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.