MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Kraton® DX421 J Linear Block Copolymer
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Kraton DX421 J is a clear, linear block copolymer based on styrene and isoprene with bound styrene of 16% mass. It is supplied from Japan. Kraton DX421 J is used in formulating adhesives, sealants and coatings. It is also used as a modifier of bitumen and polymers and in formulating compounds.

Kraton DX421 JSP supplied as dusted, dense pellet.

Information provided by Kraton Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 g/ccISO 2781
Melt Flow 2.0 - 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Typical Melt Flow at 190C/2160g is 2.8 g/10min; ISO 1133
Ash <= 1.0 %ISO 247
 
Chemical PropertiesOriginal ValueComments
Diblock Content 55 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 32
@Time 30.0 sec
ISO 7619
Tensile Strength 1310 psiISO 37
Elongation at Break 1300 %ISO 37
300% Modulus 72.5 psi
@Strain 300 %
ISO 37
 
Descriptive Properties
Volatile Matter (%m)<= 1KM 04

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKQZ9025 / 239889

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.