MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Formosa Plastics Formolene® L62022B Film (Hexene Grade) LLDPE  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: Hexene Copolymer (Barefoot)

Applications: Cast stretch film and high quality packaging films requiring clarity and toughness.

A Hexene Copolymer Linear Low Density Polyethylene for film applications including cast stretch film and high quality packaging films requiring clarity and toughness. Available with different additive packages.

Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.

Film properties measured on 20 micron cast film extruded at 1000 ft/min with a melt temperature at 510°F. Actual film properties may vary depending on operating conditions.

Information provided by Formosa Plastics Corporation, USA.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.919 g/ccASTM D1505
Thickness 20.0 microns
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Condition E; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 500 %ASTM D882
Film Elongation at Break, TD 915 %ASTM D882
Elmendorf Tear Strength, MD 295 g/milASTM D1922
Elmendorf Tear Strength, TD 628 g/milASTM D1922
Dart Drop 93.0 g/milASTM D1709
Film Tensile Strength at Break, MD 6500 psiASTM D882
Film Tensile Strength at Break, TD 5000 psiASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 1.7 %ASTM D1003
Gloss 98 %45°; ASTM D2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow AFFINITY™ PL 1840 Polyolefin Plastomer
ExxonMobil Vistamaxx™ 6202 Propylene-based Elastomer
ExxonMobil LLDPE LL 6202.19 Linear Low Density Polyethylene Resin
ExxonMobil LL 6202.19 Injection Molding Resin

PFPCPE47 / 38854

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.