MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Thermal Ceramics Superwool 607 PM Board
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Superwool 607 PM boards are processed from a slurry consisting of Superwool bulk and organic binders. This board product is noted for its excellent surface finish, thickness uniformity and high insulating value at elevated temperatures.

Superwool provides stability and resistance to chemical attack. Exceptions include hydrofluoric acid, phosphoric acid and strong alkalis (i.e. NaOH, KOH). Superwool is unaffected by incidental spills of oil or water. Thermal and physical properties are restored after drying.

The non-wetting characteristics of the Superwool 607 PM Board composition make is an excellent alternative for molten aluminium contact.

Features:

  • Continuous temperature rating of 1832°F
  • Low thermal conductivity and heat storage
  • Very close thickness tolerance
  • Excellent surface finish and uniformity
  • Easily fabricated and die-cut
  • Applications:

  • Appliance and heat processing equipment insulation
  • Combustion chamber construction for domestic appliance construction
  • Heat shields
  • High temperature gaskets and seals
  • Back-up insulation to dense refractories
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 0.240 - 0.272 g/cc
    Loss On Ignition 2.0 - 4.0 %
     
    Mechanical PropertiesOriginal ValueComments
    Modulus of Rupture 0.200 - 0.250 ksi
    Compressive Yield Strength 0.103 - 0.172 MPaat 5% deformation
     0.172 - 0.276 MPaat 10% deformation
     
    Thermal PropertiesOriginal ValueComments
    Thermal Conductivity 0.400 BTU-in/hr-ft²-°F
    @Temperature 260 °C
    ASTM C201
     0.620 BTU-in/hr-ft²-°F
    @Temperature 538 °C
    ASTM C201
     0.990 BTU-in/hr-ft²-°F
    @Temperature 816 °C
    ASTM C201
     1.31 BTU-in/hr-ft²-°F
    @Temperature 982 °C
    ASTM C201
    Melting Point 2327 °F
    Maximum Service Temperature, Air 1832 °F
    Shrinkage 1.0 %
    @Temperature 982 °C,
    Time 86400 sec
     
    Component Elements PropertiesOriginal ValueComments
    CaO 27 %
    MgO 5.0 %
    Other 1.0 %
    SiO2 67 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Zircar Zirconia ZYF-A2.13 Zirconia Felt Insulation
    Thermal Ceramics Kaowool 3000 High Temperature Board
    Thermal Ceramics 2100 RPC Shapes
    Schott ZERODUR® K20 Glass Ceramic
    Cotronics Resbond™ 919 High Temperature Ceramic Adhesive, High Resistance

    CTHERM291 / 2611

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.