Temper: Hard Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Butt Weld; Fair Suitability – Spot Weld, Capacity for Being Hot Formed Common Fabrication Processes: Blanking; Drawing; Etching; Forming and Bending; Heading and Upsetting; Piercing and Punching; Roll Threading and Knurling; Shearing; Spinning; Squeezing and Swaging; Stamping Typical uses: Medallions; Ornamental Components; Spandrels; Decorative Panels; Clock Dials; Musical Instrument Parts; Plaques; Battery Caps; Rotor Bars, AC Motors; Flexible Hose; Flexible Hose Bellows; Pump Lines; Welding Wire; Tokens Applicable Specifications: Bar – ASTM B36/B36M, ASTM B19; Brazing Filler Metal – FEDERAL QQ-B-650; Cups – ASTM B19; Plate - ASTM B36/B36M, ASTM B19; Rod, Bar & Shapes - ASTM B927/B927M; Sheet - SAE J463; ASTM B36/B36M, SAE J461; Strip - SAE J461, ASTM B36/B36M, SAE J463; Strip, Sheet & Plate – ASTM B19; Wire – ASTM B134/B134M |