MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nylene® Nylene NX4795 Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized

Material Notes: Heat stabilized, lubricated nylon 6 intended for use in coating wire, usually extrusion coated over a layer of PVC on electrical wires for toughness, temperature resistance, and insulating properties, and contains a high slip additive for ease of use when pulling wire through conduit. Delivered dry, with less than 0.2% moisture, and can be extruded as received.

Testing conducted on dry as molded specimen

Information provided by Nylene® Global Polymer Solutions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/cc
 1.23 g/cc
Water Absorption 0.12 %
Viscosity Measurement 50ASTM in 90% formic acid
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 117
Tensile Strength 30.0 MPa
@Temperature 77.0 °C
 45.0 MPa
@Temperature 77.0 °C
 61.0 MPa
@Temperature 23.0 °C
 82.0 MPa
@Temperature -40.0 °C
 82.0 MPa
@Temperature 23.0 °C
 100 MPa
@Temperature -40.0 °C
Elongation at Break 10 %
@Temperature -40.0 °C
 40 %
@Temperature -40.0 °C
 70 %
@Temperature 23.0 °C
 150 %
@Temperature 77.0 °C
 200 %
@Temperature 23.0 °C
 225 %
@Temperature 77.0 °C
Flexural Strength 26.0 MPaCond
 100 MPaDry
Izod Impact, Notched 27.0 J/m
@Temperature -40.0 °C
 28.0 J/m
@Temperature -40.0 °C
 54.0 J/m
@Temperature 23.0 °C
 220 J/m
@Temperature 77.0 °C
 320 J/m
@Temperature 23.0 °C
 800 J/m
@Temperature 77.0 °C
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.8
@Frequency 1e+7 Hz
dry
 4.7
@Frequency 10000 Hz
dry
 5.1
@Frequency 60 Hz
dry
Dielectric Strength 440 V/mil
Dissipation Factor 0.0301000
 0.0501
 0.0600.06
 
Thermal PropertiesOriginal ValueComments
CTE, linear 46.1 µm/m-°C
Melting Point 220 °Ccond
 220 °Cdry
Deflection Temperature at 0.46 MPa (66 psi) 175 °C
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
 75.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mocom (ALBIS) ALTECH® PA66 A 1000/517.01 IM Nylon 66
Taiwan Sheen Soon Sheenthane® AS-626SL TPU for PU Adhesive
Taiwan Sheen Soon Sheenthane® AH-701 TPU for Hotmelt Adhesive
SunChemical Gwent C2010517D4 Carbon/Graphite Ink
Röchling Polystone® P Grey Copolymer EHS Polypropylene + High-Temp additive

PNYLEN943 / 221475

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.