MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Michelman® Michem® Emulsion 34935 Anionic paraffin/ethylene acrylic acid wax emulsion
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Ethylene Acrylic Acid

Material Notes: Description: Anionic paraffin/ethylene acrylic acid wax emulsion

Usage: Michem® Emulsion 34935 is best used as an additive where excellent water beading properties are required It is primarily used for its water resistant properties in the wood coatings and paper coatings markets.

We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foam

Food Contact Information when manufactured in the USA:
FDA:
175.105: Components of adhesives.

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 - 0.970 g/cc
Volatiles 64.5 - 65.5 %
pH <= 7.0Recommended pH of system
 8.5 - 9.5
Brookfield Viscosity 400 - 1800 cPSpindle # 3, rpm 60
 
Descriptive Properties
AppearanceWhite, viscous liquid
Emulsifier ChargeAnionic
Solids TypeParaffin/Ethylene Acrylic Acid Copolymer blend

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Michelman® Hydrolube™ 723 Paraffin wax emulsion
BCC Products BC 83 Liquid Wax Painting/White
Michelman® Michem® Lube 723 Nonionic paraffin wax emulsion
Evonik VESTOWAX® H 2050 MG Hard Paraffin Wax
Michelman® FiberMax® 5000 Water based medium treatment to replace paraffin wax

WMICHEL078 / 134995

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.