MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Röchling Glastic 1130 Angles, Channels, and Structural Shapes
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS

Material Notes:

Information provided by Glastic Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.10 %% by wt.; ASTM D-570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 14600 psiLengthwise; ASTM D-638
 16000 psiCrosswise; ASTM D-638
Tensile Modulus 1.49e+6 psiLengthwise/Crosswise; ASTM D-638
Flexural Strength 20400 psiLengthwise; ASTM D-790
 23300 psiCrosswise; ASTM D-790
Flexural Modulus 1.39e+6 psiCrosswise; ASTM D-790
 1.41e+6 psiLengthwise; ASTM D-790
Adhesive Bond Strength 6100 psilbs.; NEMA 11.11
Izod Impact, Notched 11.3 ft-lb/inASTM D-256
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 12.4 kV/mmPerpendicular S/T in Air; ASTM D-149
Arc Resistance 192 secASTM D-495
Track Resistance 52200 secInclined Plane; ASTM D-2303
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0
Flame Spread Index 12Radiant Panel; ASTM E-162
 20UL Standard 723; ASTM E-84
 
Descriptive Properties
Electric Strength kV, ASTM D14975Parallel, Condition A
 79Parallel, Condition D (48/50)
Smoke Developed115ASTM E-84
Standard ColorGray
UL Recognition File NumberR9599
UL Standard 723 Fuel Contributed0ASTM E-84

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM A709 Steel, grade 50, high-strength, low alloy steel (≤ 50 mm)
ASTM A285, Grade A
ASTM A516, Grade 55
ASTM A514 Steel, grade P, plate thickness ≤ 19 mm
AISI E9310H Steel, normalized, machined to 25 mm (1 in.) rounds, pseudocarburized, 150°C (300°F) temper

PGLASX2 / 41946

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.