MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess LEWATIT® A 365 Polyacrylate Anion Exchange Resin
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Lewatit® A-365 > is a food grade, macroporous, weakly basic anion exchange resin based on a crosslinked polyacrylate. Lewatit A-365 is designed to offer exceptional high operating capacity, good physical stability and excellent resistance to mechanical osmotic shock. The acrylic matrix of Lewatit A-365 offers rapid kinetics for common anions, including larger, more bulky, anions like sulfate. Lewatit A-365 is fully regenerable with NaOH and other weak bases. As Lewatit A-365 is a true weak base resin, the regenerant consumption is close to stoichiometric. Lewatit A-365 is recommended for applications including demineralization of high TDS waters, selective sulfate removal, purification of aqueous solutions, including decolorization applications and once-through cartridge applications. Lewatit A-365 is supplied in a heterodispersed particle size distribution as spherical beads in the fully swollen moist free base form. Lewatit A-365 is prepared with a minimum amount of fines (-50 mesh particles) resulting in low pressure losses during service.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.730 g/cc
Density 1.13 g/cc
Volatiles <= 0.60 %
@Temperature 105 °C,
Time 21600 sec
ISO 248/ASTM D5668
Bead Size 0.400 - 1.25 mm>90%
Mooney Viscosity 32 - 44
@Temperature 100 °C
(1+4); ISO 289/ASTM D1646
Vinyl Acetate Content 88 - 92 %
Storage Temperature -20.0 - 40.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 60.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceYellow-white, opaque
pH Operating Range0 - 9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8728 / 209121

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.