MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECATEC PA66 GW43 PL S0001 black - plate Nylon 66, Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled

Material Notes: Fillers: glass fibers

Main features:

  • very good abrasion resistance
  • electrically insulating
  • very good mechanical strength
Target Industries:
  • automotive industry
  • mechanical engineering
  • oil and gas industry
  • safety engineering
  • sporting goods

Information provided by Ensinger Composites.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 350 MPaISO 527-4
Tensile Modulus 21.0 GPaISO 527-4
Flexural Strength 316 MPaISO 14125
Flexural Modulus 20.8 GPaISO 14125
Shear Strength 26.0 MPainterlaminar; ISO 14130
 54.0 MPainterplanar; ISO 14129
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µm/m-°Cin 0° and 90° direction
Melting Point 260 °C
Maximum Service Temperature, Air 110 °Clong term
 180 °Cshort term
Glass Transition Temp, Tg 47.0 °C
 
Descriptive Properties
Areal weight finished product449 g/m²
Colorblack
Fiber architectureTwill 2/2
Fiber areal weight280 g/m²
Fiber orientation0-90°
Fiber typeE glass
Fiber volume content0.43
Layers1-95
Material widths625x525 mm
Resin weight content0.377

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIN520 / 287744

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.