MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: Anviloy® 1150 is a tungsten-based material that was developed primarily for die-casting, aluminum permanent mold, and difficult extrusions. It is produced by a high temperature powder metallurgy processes. A low coefficient of thermal expansion, good thermal conductivity and good material properties at elevated temperatures combine for superior performance in a variety of applications. This unusual combination of properties results in less thermal fatigue and soldering in the die cast or extrusion

Applications:

  • Die Cast Tooling
  • Extrusion Dies
  • Hot Runner Nozzles
  • Vibration and Tool Chatter Reduction
  • Plastic Injection Molding
  • High Elongation Requirements
  • Maximum Thermal Conductivity Needs
  • Shot Sleeves

Astaras, Inc. purchased the entire Anviloy® business from CMW in 2014. Information provided by Astaras, Inc.

Key Words: Powder Metallurgy (P/M)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 17.25 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 34
Hardness, Vickers 335HV10
Tensile Strength, Ultimate 517 MPa
@Temperature 816 °C
 724 MPa
@Temperature 649 °C
 779 MPa
@Temperature 538 °C
 950 MPa
@Temperature 22.2 °C
Tensile Strength, Yield 650 MPa
Elongation at Break >= 10 %in 2 in (51 mm)
Modulus of Elasticity 338 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.53 µm/m-°C
@Temperature 20.0 - 400 °C
 5.26 µm/m-°C
@Temperature 20.0 - 800 °C
Thermal Conductivity 70.2 W/m-K
Melting Point 1425 - 3410 °C
Solidus 1425 °C
Liquidus 3410 °C
 
Component Elements PropertiesOriginal ValueComments
Iron, Fe 2.0 %
Molybdenum, Mo 4.0 %
Nickel, Ni 4.0 %
Tungsten, W 90 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Astaras Anviloy® Weld Rod
Kennametal Densalloy™ SD170
Titanium, Ti
Aluminum 357.0-F Casting Alloy
Mi-Tech Metals Super Chatter Free™ HD17.7 Tungsten-Based Metal

NCMW00 / 15872

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.