MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
FKuR Kunststoff Terralene® LL 1303 Biobased Polyethylene
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol used for Green PE is not produced using crude oil, but instead is derived from sugarcane. Therefore each ton of Green PE captures up to 2.5 tons of CO2 thus helping to reduce harmful greenhouse gas emissions. As Terralene® offers the same characteristics and processability as fossil polyethylene it is a drop-in replacement and can be run on conventional PE production equipment. This allows Terralene® to help meet sustainability goals affordably. Furthermore, Terralene® is 100% recyclable using standard Polyethylene recycling streams. With its unique technology FKuR increases the range of applications for Green PE particularly for injection moulded components and film.

Terralene® - for Flexible Applications and Extrusion Coating

Green LLDPE and HDPE can have a limited range of applications. Terralene® can provide a perfect answer as these grades produce high quality films with a well-designed and full additive package. Terralene® is FKuR’s solution to complete their current Green PE portfolio achieving LDPE like properties and behaviour. Due to the excellent homogeneity and blend of polymers, Terralene® provides simple gel-free production. For extrusion coating, Terralene® has a low neck-in with a good draw down ratio.

Terralene® - for Injection Molding

With good flow properties and melt strength, Terralene® provides the desirable characteristics required for the moulding of complex structures. The performance of Green PE is often limited to pure HDPE applications, however Terralene® extends the range of applications and is FKuR’s solution for optimizing the processing and product performance while still catering to individual requirements.

TERRALENE® LL 1303 is ideal for extrusion coating and lamination. Using a unique combination of additives, TERRALENE® LL 1303 offers excellent procesability along with a reduction of the neck-in when compared to pure Green PE. Furthermore, TERRALENE® LL 1303 stands out as it has a high natural resource content and mechanical properties which are similar to LDPE.

Information Provided by FKuR Kunststoff GmbH
Key Words: LDPE, HDPE, butene copolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.919 g/ccISO 1183
Melt Flow 2.4 - 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 14.0 MPaISO 527
Tensile Strength, Yield 15.0 MPaISO 527
Elongation at Break 480 %ISO 527
Elongation at Yield 475 %ISO 527
Tensile Modulus 200 MPaISO 527
Flexural Yield Strength 5.70 MPa
@Strain 3.5 %
ISO 178
Flexural Modulus 0.180 GPaISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179-1/1eU
Charpy Impact, Notched 68.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 130 - 145 °CISO 3146-C
Vicat Softening Point 95.0 °CA; ISO 306
 
Descriptive Properties
Flexural strain at break (%)No BreakISO 178
Melt Volume Flow (cm3/10 min)3.2-4.0ISO 1133; 190°C, 2.16kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SK Chemicals SKYTHANE® SG400 SKYGREEN Biodegradable Thermoplastic
Eastman Tenite 285A2R30020 Cellulose Acetate Butyrate, Natural, Trsp
EMS-Grivory Grilamid® XE 4116 nat PA1010-GF55
RTP Company RTP 199 X 143685 A Polypropylene (PP); Copolymer - Cellulose Fiber - 20% Renewable Resource Content
RTP Company RTP 2099 X 121241 B Bio-Based Polylactic Acid (PLA); PC-PLA Blend - ESD Protection - Permanently Anti-static - 26% Renewable Resource Content

PFKUR021 / 138491

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.