MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Vespel® CR-4638 Thermoplastic Parts and Shapes
Categories: Polymer; Thermoplastic

Material Notes: Vespel® CR-4638 parts use the latest reinforced, chemically resistant, thermoplastic polymer. Custom parts molded from CR-4638 resin help provide electrical conductivity to dissipate accumulated static charges, resulting in lower particle generation. CR-4638 material also offers improved wear resistance for longer part life. Customers have reported that these characteristics are beneficial in a variety of applications, including semiconductor wafer handling. Traditional thermoplastic processing methods can be employed to produce custom parts with CR-4638.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.42 g/ccASTM D792
Water Absorption 0.060 %24 hrs @ 73°F.; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 40ASTM D785
Tensile Strength 142 MPaISO 527
Elongation at Break 1.0 %ISO 527
Tensile Modulus 21.1 GPaISO 527
Flexural Strength 216 MPaISO 178
Flexural Modulus 19.7 GPaISO 178
Izod Impact, Notched (ISO) 5.03 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) 20.0 kJ/m²ISO 180
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 10000 ohm-cm - 1e+05ASTM D4496
Surface Resistance 10000 ohm - 1e+05IEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 6.60 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 48.5 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 157 °CISO 75F
Deflection Temperature at 1.8 MPa (264 psi) 151 °CISO 75F
Glass Transition Temp, Tg 154 °CDMA
Flammability, UL94 V-0
@Thickness 3.20 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDU2000_copy / 293405

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.