MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
3M Techical Ceramics Titanium Diboride
Categories: Ceramic; Boride

Material Notes:

Information provided by 3M Technical Ceramics, formerly ESK Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 4.50 g/ccDIN EN 623-2
Porosity <= 1.5 %DIN EN 623-2
Weibull Modulus 16[m]; DIN EN 843-5
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 25.6
@Pressure 100 MPa
DIN EN 843-4
Tensile Modulus 575 GPaYoung's; DIN EN 843-2
Flexural Strength 500 MPaDIN EN 843-1
Poissons Ratio 0.11
Fracture Toughness 8.00 MPa-m½SENB
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000200 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.70 µm/m-°C
@Temperature 20.0 - 500 °C
DIN EN 821-1
 8.20 µm/m-°C
@Temperature 500 - 1000 °C
DIN EN 821-1
Thermal Conductivity 54.0 W/m-K
@Temperature 50.0 °C
DIN EN 821-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
H.C. Starck Grade F Titanium Diboride, TiB2
Momentive Performance Materials HCT-30D Titanium Diboride (TiB2) Powder
H.C. Starck Grade D Titanium Diboride, TiB2
Ceradyne Ceralloy® 225 Titanium Diboride
Goodfellow Titanium Diboride, TiB2

CESK23 / 183315

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.