Sandvik 19.12.3.LR CRYO is a covered chromium nickel electrode with rutile basic coating for welding of steels of ASTM 316L base materials for cryogenic applications. The electrode has excellent arc stability and fast burn off rate with minimal stub loss. It is also characterized by improved moisture resistance, self peeling slag and easy post weld finishing. Sandvik 19.12.3.LR CRYO gives smooth uniform beads and works in any standard weld position.Information provided by Sandvik |