MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Skamol Group SKAMOCAST 112-80 Insulating Castable  (discontinued **)
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: SKAMOL insulating castables have the following characteristics:
  • Max. service temperature: Up to 1100°C (2102°F)
  • Back-up insulation or hot-face uses
  • For casting and gunning
  • Products are based on fired Moler aggregates, refractory materials, or exfoliated vermiculite
  • Effective insulation
  • Quick and economical installation
  • Used as monolithic heat insulation in a wide range of industrial kilns and furnaces, boilers, chimneys, and flues
  • The Vermicast grades are favored as infill in aluminum reduction cell cathodes due to their non-wetting capacity to molten metal and good bath resistance.

Information provided by Skamol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 34.0 lb/ft³As Supplied
 50.0 lb/ft³Defined by casting method, +/- 50kg (110 lbs)
Loss On Ignition 6.0 %
@Temperature 1025 °C
Porosity 68 %
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 2.90 MPaDried at 110°C (230°F)
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.200 W/m-K
@Temperature 200 °C
Mean temp.; ASTM C-201 supplemented by ASTM C-182
 0.220 W/m-K
@Temperature 400 °C
ASTM C-201 supplemented by ASTM C-182
 0.240 W/m-K
@Temperature 600 °C
ASTM C-201 supplemented by ASTM C-182
Maximum Service Temperature, Air 900 °C
Shrinkage 1.5 %
@Time 43200 sec
Linear Reheat Shrinkage, 12h at 100°C (180°F) below max. service temp.
 
Component Elements PropertiesOriginal ValueComments
Al2O3 + TiO2 14.5 %
CaO 7.0 %
Fe2O3 8.0 %
K2O+Na2O 1.0 %
MgO 1.0 %
SiO2 62 %
 
Descriptive Properties
Pyrometric Cone Equivalent1200°CASTM C24-89, ORTON cones

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CSKAM028 / 2179

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.