MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

(Viewing data as-entered. Click here to return)
HP Alloys Alloy 718, 30% Cold Worked
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.

Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes International.

Key Words: NACE MR-01-75, ASTM B626; AFNOR NC 19 Fe Nb, UNS N07718, AMS 5596, AMS 5597, AMS 5662, AMS 5664, AMS 5832, AMS 5589, AMS 5590, Werkstoff Nr. 2.4668; WL Nr. 2.4668; MIL-N-24469; NACE MR-01-75; AECMA Pr EN 2404, 2405, 2407, 2408, 2952, 2961, 3219
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.20 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1331 MPa
Tensile Strength, Yield 1241 MPa
Elongation at Break 15 %
Reduction of Area 46 %
Modulus of Elasticity 200 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000123 ohm-cm
Magnetic Permeability 1.0011at 200 Oersted (15.9 kA/m)
Curie Temperature -112 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.9 µm/m-°C
@Temperature 20.0 - 100 °C
 13.5 µm/m-°C
@Temperature 25.0 - 200 °C
 14.3 µm/m-°C
@Temperature 25.0 - 500 °C
 17.2 µm/m-°C
@Temperature 25.0 - 900 °C
Specific Heat Capacity 0.435 J/g-°C
Thermal Conductivity 11.4 W/m-K
Melting Point 1260 - 1336 °C
Solidus 1260 °C
Liquidus 1336 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.20 - 0.80 %
Boron, B <= 0.0060 %
Carbon, C <= 0.080 %
Chromium, Cr 17 - 21 %
Cobalt, Co <= 1.0 %
Copper, Cu <= 0.30 %
Iron, Fe 17 %
Manganese, Mn <= 0.35 %
Molybdenum, Mo 2.8 - 3.3 %
Nickel, Ni 50 - 55 %
Niobium, Nb (Columbium, Cb) 4.75 - 5.5 %
Phosphorus, P <= 0.015 %
Silicon, Si <= 0.35 %
Sulfur, S <= 0.015 %
Titanium, Ti 0.65 - 1.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
HP Alloys Alloy 718, 5% Cold Worked
HP Alloys Alloy 718, 50% Cold Worked
HP Alloys Alloy 718, 20% Cold Worked
HP Alloys Alloy 718, 30% Cold Worked, Aged
HP Alloys Alloy 718, 0% Cold Worked, Not Aged

NPH716 / 18793

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.