MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Ohara WMS-15 Glass Ceramic Substrate
Categories: Ceramic; Machinable Ceramic

Material Notes: WMS-15 glass-ceramic substrates enable production of DWDM and Gain-Flattening Filters. WMS substrates facilitate the production of filters with extremely low thermal wavelength drift and low insertion loss values. WMS-15 has improved internal transmittance and exceptionally low surface roughness values. It is superior for machining - less edge chipping on the filters than amorphous glass substrates. It has a very high thermal expansion coefficient and excellent chemical resistance.

Information provided by Ohara Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 800
Modulus of Elasticity 96.0 GPa
Abrasion 31Aa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.4 µm/m-°C
@Temperature -30.0 - 70.0 °C
Thermal Conductivity 1.90 W/m-K
Maximum Service Temperature, Air 650 °CHeat Resistance
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.524
@Wavelength 1550 nm
IR Transmittance 99.9 %
@Thickness 1.00 mm,
Wavelength 1550 nm
 
Component Elements PropertiesOriginal ValueComments
Alkalis 10.9 %
 
Descriptive Properties
Acid Resistance, Powder Method, RA(P)1
Water Resistance, RW(P)1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CZOHARA788 / 281627

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.