Daplen EE109AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE109AE is a material with excellent impact /stiffness ratio. Thanks to its low thermal expansion this material is suitable to mold parts requiring low change of dimensions over a broad temperature range. This product is optimized to give good surface aesthetics. Daplen EE109AE has been developed especially for bumpers, body side molding, and body panels. Information provided by the Manufacturer. |