MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene GA652962 High Density Polyethylene (HDPE), Rotational Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Rotational Molding Grade

Material Notes: Petrothene GA652962 is a hexene HDPE resin selected for rotationally molding large tank applications. GA652962 is UV-stabilized and is available in a 35 mesh powder as Microthene MP652962. Applications: Containers, Intermediate Bulk Containers, Tanks, Industrial

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.942 g/ccASTM D1505
ESCR 100% Igepal® >= 400 hourCond. A; ASTM D 1693
ESCR 10% Igepal® >= 50 hourCond. A; ASTM D 1693
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 23.4 MPaASTM D638
Flexural Modulus, 1% Secant 1010 MPaASTM D790
2% Secant Modulus 855 MPaASTM D790
Impact Test 55.0 J
@Temperature -40.0 °C
1/4" specimen, ARM
 215 J
@Temperature -40.0 °C
1/4" specimen, ARM
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 43.0 °Cunannealed; ASTM D648
 65.0 °Cunannealed; ASTM D648
 
Descriptive Properties
Processing MethodRotomolding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Microthene MP652962 HDPE
Braskem RC35U4 LLDPE Rotomolding Polyethylene
Braskem ML4400N LLDPE Rotomolding Polyethylene
ExxonMobil LLP8460.29 Rotational Molding Resin
LyondellBasell Petrothene PM96750

PEQT8832 / 220466

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.