MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Chemours Krytox® XHT-500 Extreme High Temperature PFPE Oil  (discontinued **)
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: These oils are a special extreme high temperature grade with low oil evaporation and have had extra treatment to allow use at temperatures above the range of normal PFPE oils. It has excellent lubrication over a broad temperature range. Krytox® XHT series oils are nonflammable and chemically inert. Krytox® allows extended lubrication intervals and longer equipment life. The oil can begin to slowly degrade at temperatures above 330°C (625°F), and this will occur at an increasing rate as temperatures increase. Relubrication could be required at these temperatures to achieve optimum life. Krytox® PFPE oils are clear, colorless, fluorinated synthetic oils that are nonreactive, nonflammable, safe in chemical and oxygen service, and are long lasting. Krytox® is a perfluoropolyether (PFPE)— also called perfluoroalkylether (PFAE) or perfluoropolyalkylether PFPAE). The polymer chain is completely saturated and contains only carbon, oxygen, and fluorine. On a weight basis, a typical Krytox® oil contains 21.6% carbon, 9.4% oxygen, and 69.0% fluorine.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Performance Lubricants, in 2015. This specific product was discontinued prior to the formation of Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.78 g/cc
@Temperature 100 °C
 1.95 g/cc
@Temperature 0.000 °C
Viscosity Measurement 148Base Oil Viscosity Index
Kinematic Viscosity 1712 cSt
@Temperature 20.0 °C
Kinematic Viscosity at 40°C (104°F) 500 cSt
Kinematic Viscosity at 100°C (212°F) 46.4 cSt
Vapor Pressure Test <= 1.00e-9 torr20°C; Knudsen
 <= 8.00e-7 torr100°C; Knudsen
 <= 0.000100 torr200°C; Knudsen
Evaporation Loss 0.80 %Oil Volatility; 22 hr; 260°C
 <= 1.0 %Oil Volatility; 22 hr; 204°C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °C
Minimum Service Temperature, Air -20.0 °C
Pour Point -25.0 °CBase Oil
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 21.6 %
Fluorine, F 69 %
Oxygen, O 9.4 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Krytox® NRT 8904 PFPE Lubricant
Chemours Krytox® NRT 8906 PFPE Lubricant
Chemours Krytox® 1645 Vacuum Service Fluid
Chemours Krytox® 16256 Vacuum Pump Fluid
Chemours Krytox® 1531XP Vacuum Pump Fluid with Antirust Protection

WDUPK00 / 75360

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.