MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos Nova PS 2521 Crystal Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Information provided by Nova Chemicals

INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D955
Melt Flow 7.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
old Condition G; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 62ASTM D785
Tensile Strength at Break 47.0 MPaASTM D638
Elongation at Break 2.0 %ASTM D638
Tensile Modulus 3.41 GPaASTM D638
Flexural Strength 96.0 MPaat <5%; ASTM D790
Flexural Modulus 3.30 GPaASTM D790
Izod Impact, Notched 21.0 J/m
@Diameter 3.17 mm
bar; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.59
@Frequency 1e+6 Hz
Dielectric Strength 500 kV/in
@Thickness 3.17 mm
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 100 °Cannealed; ASTM D648
Vicat Softening Point 91.0 °CRate B; ASTM D1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.59 - 1.60
@Wavelength 589.3 nm
Sodium D Line
Optical Density 0.046400 mm- 700 mm average
Transmission, Visible 88 - 90 %
@Wavelength 550 nm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 190 - 274 °C
Mold Temperature 38.0 - 82.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chi Mei Polylac® PA-746Y ABS
Techmer ES Plastiblend® PC/ABS 88 GF 10% Glass Filled
MRC Polymers NAXELL™ PC110MH General Purpose Medium High MFR Polycarbonate
Ineos Nova PS 3190 Crystal Polystyrene
Covestro Makrolon® 6265 Polycarbonate, Flame Retardant Grade

PNOV901 / 54847

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.