MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
The Chemical Company ChemFlexx™ 206 Phthalate Plasticizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemflexx 206 is considered to be a “functional replacement” for linear plasticizers. It is an organic, non-hazardous, liquid, phthalate ester. Chemflexx 206 is a plasticizer for the manufacture of flexible plastics. End use applications include PVC floor coverings, roofing membranes, swimming pool liners and wall coverings, expanded leather, PVC foams, films, sealing and adhesive systems based on poly urethane or polysulphide, soft squeeze toys, balls, vinyl upholstery, tablecloths, shower curtains, raincoats, and a range of other products that must stay flexible for the lifetime of their use.

Information provided by The Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.966 - 0.977 g/cc
@Temperature 20.0 °C
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.010parent acid %
 <= 0.070mg KOH/g
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8115 sec. delay
 87Instant
Tensile Strength, Ultimate 2391.2 psioven aged 7 days @ 113°C
 2440 psi
 2440 psioven aged 10 days @ 100°C
Elongation at Break 329 %oven aged 7 days @ 113°C
 354 %
 354 %oven aged 10 days @ 100°C
100% Modulus 1.959 ksi
@Strain 100 %
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -30.5 °C
Oxygen Index 30 %
 
Descriptive Properties
Alcohol Content= 1000ppm
AppearanceClear and free of suspended matter
Assay= 99.6%
Hazen Color Value (pt-co)= 35
Weight Loss (%)1oven aged 10 days @ 100°C
 4oven aged 7 days @ 113°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTCC003 / 106992

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.